Fire Retardant Steel Cord Conveyor Belt
Our fire retardant conveyor belts are widely utilized in fiery mines whereby the compound and carcass is suppressed to significantly reduce or
Overlay performance and level | |||
Tensile strength | ≥ 15Mpa | ||
Elongation at break: | ≥350% | ||
Aging test: | (70℃ x 168h) | ||
Change rate of tensile strength: | -25 ~ +25% | ||
Change rate of elongation at break: | -25 ~ +25% | ||
Abrasion | ≤ 200mm³ | ||
Safety performance | |||
Item | Index | ||
Guide | Average value of the upper and lower sides of the upper and lower | 3≤10^8 | |
Roller Friction | Roller surface temperature | ≤325 | |
There is no clear flame and no flame burning | |||
Alcohol burner combustion | Complete cover layer combustion | The average value of the 6 samples was. S | ≤3 |
The average value of the 6 samples was. S | ≤10 | ||
a flame or flame | Cover layer | The average value of the 6 samples was. S | ≤5 |
The average value of the 6 samples was. S | ≤15 | ||
Propane burner | No burn length | ≥250MM |